Skip navigation

DSpace JSPUI

DSpace preserves and enables easy and open access to all types of digital content including text, images, moving images, mpegs and data sets

Learn More
DSpace logo
English
中文
  • Browse
    • Communities
      & Collections
    • Publication Year
    • Author
    • Title
    • Subject
  • Search TDR
  • Rights Q&A
    • My Page
    • Receive email
      updates
    • Edit Profile
  1. NTU Theses and Dissertations Repository
  2. 工學院
  3. 環境工程學研究所
Please use this identifier to cite or link to this item: http://tdr.lib.ntu.edu.tw/jspui/handle/123456789/28083
Title: 機車使用觸媒熱劣化現象之探討
Thermal Deactivation of Catalyst Converters on Motorcycles
Authors: Yi-Hsien Yu
余奕賢
Advisor: 鄭福田(Fu-Tien Jeng)
Keyword: 三元觸媒轉化器,實驗室加速劣化程序,熱劣化,活性測試,起燃溫度曲線,熱劣化預測模式,
three-way catalyst,laboratory scale aging,thermal deactivation,activity test,light-off curve,thermal deactivation,predictive model,
Publication Year : 2007
Degree: 碩士
Abstract: 機車為我國廣為應用之交通工具,然而以往移動源研究對象以汽車為多,機車相關研究十分有限。以往探討三元觸媒轉化器劣化機制
之研究,亦多侷限以汽車為對象。有鑑於此,本研究利用配製模擬廢氣及實驗室加速劣化程序,檢討操作溫度、操作時間及廢氣含氧量對三元觸媒轉化器之影響。本研究利用排氣分析儀配製模擬廢氣通入觸媒中並加以高溫進行劣化程序,再將經劣化後之觸媒樣品,進行特性分析及相關檢討。
觸媒因高溫操作導致熱劣化之機制主要分為載體燒結、活性金屬
燒結及具有活性之結晶因高溫轉變成不具活性。由比較面積分析儀、X光粉末繞射儀、掃瞄式電子顯微鏡—能量分散光譜儀分析結果顯示:在機車操作溫度範圍內,主要熱劣化機制為載體燒結,不論在何種劣化條件下,觸媒之比表面積及孔徑分佈隨劣化溫度提高而往低比表面積及大孔徑分佈方向成長。
在不同劣化條件劣化之觸媒,其起燃溫度曲線呈現不同特性的改變,經5 小時劣化之觸媒活性測試結果與其他條件劣化之觸媒呈趨勢不規則之變化。經當量點及氧化性劣化之觸媒活性測試結果相似,而經還原性劣化之觸媒,活性指標T75 優於其餘二者。溫度與廢氣含氧量對觸媒熱劣化影響較劣化時間顯著。在本研究設定之劣化條件範圍內,本研究建構之模式可合理推估觸媒經長時間操作後之比表面積變化情形。
Motorcycles constitute important parts of air pollution emission in Taiwan. However, only limited studies were focused on the deactivation mechanisms of three-way catalyst converters used in motorcycles.
Furthermore, the performance of deactivated catalyst converters on motorcycles has not been extensively studied. In this study, thermal aging of the catalyst is simulated in laboratory scale. Based on results of
several surface characterization techniques, the effects of aging test exhaust, temperature, and time were examined.
Thermal deactivation mechanism is a combination of several aging phenomena, including sintering of active phase, the collapse in surface area and the thermal deactivation of solid phase. According to the measurement results of specific surface area, XRPD, SEM-EDS, the main mechanism of thermal deactivation is deduced as the collapse in surface area. For all thermal aging operating modes studied, the temperature increase reduced the specific surface area and increased the pore size.
For all thermal aging operating modes studied, light-off curves of aged catalysts were different. The activity test results of 5 hours aged catalysts were differ from others. The results of activity test of during stochiometric and oxidative aging were similar, and the activity indicator,
T75 of during reductive aging catalysts, was lower than the others. The aging temperature and composition of test exhaust are more effective than aging time. The constructed model has good performance on predictions within the thermal aging operating range studied.
URI: http://tdr.lib.ntu.edu.tw/jspui/handle/123456789/28083
Fulltext Rights: 有償授權
Appears in Collections:環境工程學研究所

Files in This Item:
File SizeFormat 
ntu-96-1.pdf
  Restricted Access
15.54 MBAdobe PDF
Show full item record


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

社群連結
聯絡資訊
10617臺北市大安區羅斯福路四段1號
No.1 Sec.4, Roosevelt Rd., Taipei, Taiwan, R.O.C. 106
Tel: (02)33662353
Email: ntuetds@ntu.edu.tw
意見箱
相關連結
館藏目錄
國內圖書館整合查詢 MetaCat
臺大學術典藏 NTU Scholars
臺大圖書館數位典藏館
本站聲明
© NTU Library All Rights Reserved