Skip navigation

DSpace

機構典藏 DSpace 系統致力於保存各式數位資料(如:文字、圖片、PDF)並使其易於取用。

點此認識 DSpace
DSpace logo
English
中文
  • 瀏覽論文
    • 校院系所
    • 出版年
    • 作者
    • 標題
    • 關鍵字
    • 指導教授
  • 搜尋 TDR
  • 授權 Q&A
    • 我的頁面
    • 接受 E-mail 通知
    • 編輯個人資料
  1. NTU Theses and Dissertations Repository
  2. 電機資訊學院
  3. 電子工程學研究所
請用此 Handle URI 來引用此文件: http://tdr.lib.ntu.edu.tw/jspui/handle/123456789/97831
完整後設資料紀錄
DC 欄位值語言
dc.contributor.advisor胡振國zh_TW
dc.contributor.advisorJenn-Gwo Hwuen
dc.contributor.author藍柏皓zh_TW
dc.contributor.authorPo-Hao Lanen
dc.date.accessioned2025-07-18T16:06:19Z-
dc.date.available2025-07-19-
dc.date.copyright2025-07-18-
dc.date.issued2025-
dc.date.submitted2025-06-26-
dc.identifier.citation[1] P.K Chang and Jenn-Gwo Hwu. Electrical characterization of 4H-SiC metal–oxide–semiconductor structure with Al2O3 stacking layers as dielectric. Applied Physics, 2018. doi: 10.1007/s00339-017-1535-8.
[2] Renbing Wu, Kun Zhou, Chee Yoon Yue, and Yi Pan Jun Wei. Recent progress in synthesis, properties and potential applications of Sic nanomaterials. Progress in Materials Science, 2015. doi: 10.1016/j.pmatsci.2015.01.003.
[3] Christian D. Matthusa, Anton J. Bauera, Lothar Freya, and Tobias Erlbachera. Wavelength-selective 4H-SiC UV-sensor array. Materials Science in Semiconductor Processing, 2019. doi: 10.1016/j.mssp.2018.10.019.
[4] Choyke W.J and Pensl G. Physical Properties of SiC. MRS Bulletin, 1997. doi:10.1557/S0883769400032723.
[5] S. K Gupta and J Akhtar. Thermal oxidation of silicon carbide (SiC)–experimentally observed facts. Silicon Carbide-Materials, Processing and Applica‐tions in Electronic Devices, 2011.
[6] J. Roy, S. Chandra, S. Das, and S. Maitra. Oxidation Behaviour Of Silicon Carbide - A Review. Rev. Adv. Mater. Sci, 2014.
[7] I Vickridge, J Ganem, Y Hoshino, and I Trimaille. Growth of SiO2 on SiC by dry thermal oxidation: mechanisms. Journal of Physics D: Applied Physics, 2007.
[8] Wei-Chi Liao and Jenn-Gwo Hwu. Low Interface Trap Density 4H-SiC MIS Structure With SiO2 Grown by Sub-1000 ◦C Intermittent Spray Hydrated Oxidation (ISHO) for UV Sensor Applications. IEEE Transactions on Electron Devices, pages 1–7, 2024. doi: 10.1109/TED.2024.3486258.
[9] Z. Zhang, Y. Guo, and J. Robertson. Mobility degradation in 4H-SiC MOSFETs and interfacial formation of carbon clusters. Solid-State Electronics, 183:108051,2021.
[10] Takahide Umeda, T. Kobayashi, Mitsuru Sometani, H. Yano, Yu ichiro Matsushita, and S. Harada. Carbon dangling-bond center (carbon Pb center) at 4H-SiC(0001)/SiO2 interface. Applied Physics Letters, 116:071604, 2020.
[11] A. Tataroglu and S.Altindal. Analysis of electrical characteristics of Au/SiO2/n-Si (MOS) capacitors using the high–low frequency capacitance and conductance methods. Microelectronic Engineering, 2008. doi: 10.1016/j.mee.2008.07.001.
[12] Wei-Chi Liao and Jenn-Gwo Hwu. Oxidation Process Development and Device Applications in 4H-SiC MIS Structure. doi: 10.6342/NTU202401607.
[13] C.‐ Y. Hu, D. L. Kencke, S. Banerjee, B. Bandyopadhyay, E. Ibok, and S. Garg. Determining effective dielectric thicknesses of metal‐oxide‐semiconductor structures in accumulation mode. Applied Physics Letters, 1995. doi:10.1063/1.113877.
[14] Yen-Po Lin and Jenn-Gwo Hwu. Using Anodization to Oxidize Ultrathin Aluminum Film for High-k Gate Dielectric Application. Journal of The Electrochemical Society, 2003. doi: 10.1149/1.1577545.
[15] Mario Curiel, Nicola Nedev, and Judith Paz. UV Sensitivity of MOS Structures with Silicon Nanoclusters. Sensors, 2019. doi: 10.3390/s19102277.
[16] Nasiri-N Bo and Tricoli A. Structural engineering of nano‐grain boundaries for low‐voltage UV‐photodetectors with gigantic photo‐to dark‐current ratios.Advanced Optical Materials, 2016.
[17] Chengchao He, Yanhong Li, Yuxiang Yang, Huaikun Fan, Dawei Li, and Xue Han. Sensitive Aluminum SPR Sensors Prepared by Thermal Evaporation Deposition. ACS Omega, 2023. doi: 10.1021/acsomega.3c06855.
[18] Po-Hao Lan and Jenn-Gwo Hwu. Reduction of leakage and interface trap density in Al/Al2O3/SiO2/4H-SiC(n) Mos structure by Low Thermal Budget Anodization Technique. International Electron Devices Materials Symposium 2024, Aug 2024.
[19] Feiyang Zhao, Yongjie He, Bin Huang, Tianyi Zhang, and Hao Zhu. A review of diamond materials and applications in power semiconductor devices. Materials, 17(14), 2024.
[20] Arnar M. Vidarsso and Jordan R. Nicholls. Detection of near-interface traps in NO annealed 4H-SiC metal oxide semiconductor capacitors combining different electrical characterization methods. Journal of Applied Physics, 2022.
[21] A. TAUBE and M. GUZIEWICZ. Characterization of Al2O3/ 4H-SiC and Al2O3/SiO2/ 4H-SiC MOS structures. BULLETIN OF THE POLISH ACADEMY OF SCIENCES, 2016.
[22] F. Arith, J. Urrcsti, K. Vasilevskiy, S. Oisenl, N. Wright, and A. O’Neill. High mobility 4H-SiC mosfet using a thin SiO2/Al2O3 gate stack. In 48th European Solid-State Device Research Conference (ESSDERC), pages 30–33, 2018.
[23] Ting-Wei Liu, Zhe Zhao, Ruyue Cao, Yue-Yang Liu, and Xiangwei Jiang. Reliability challenges of gate dielectric materials in transistors. Information & Functional Materials, 2(1):62–92, 2025.
[24] Yu-Dong Lv, Lei Shen, Yu-Chun Li, Cai-Yu Shi, Zi-Ying Huang, Xing Yu, Xiao-Na Zhu, Hong-Liang Lu, Shaofeng Yu, and David Wei Zhang. Atomic-Layer-Deposited Al2O3 Layer Inserted in SiO2/HfO2 Gate-Stack-Induced Positive Flat-Band Shift with Dual Interface Dipoles for Advanced Logic Device. ACS Applied Nano Materials, 7(24):28496–28503, 2024.
-
dc.identifier.urihttp://tdr.lib.ntu.edu.tw/jspui/handle/123456789/97831-
dc.description.abstract本研究主要探討陽極氧化氧化鋁與閘極絕緣層於碳化矽基板上的製程與應用。首先,研究分析了紫外光源照射對於陽極氧化的影響。結果顯示,在紫外燈照射下進行陽極氧化能夠促進碳化矽基板中電洞的產生,進而提升陽極氧化電流,並增強二氧化矽層的成長效率,此方法成功製備出厚度達16 奈米均勻的二氧化矽層。
本研究亦探討了間歇式噴霧水合氧化法及其改良版本── 重複噴霧式間歇水合氧化法在碳化矽基板上形成二氧化矽層的特性。結果顯示,重複噴霧式間歇水合氧化法可在950◦C 下形成厚度為3至6 奈米的均勻且緻密的二氧化矽薄膜,具有低漏電流的優勢。由電容-電壓特性,重複噴霧式間歇水合氧化法所成長的氧化層在碳化矽介面上的介面陷阱密度低至5×10^11 cm^−2 eV^−1。在不同紫外光強度下偏壓於-6 V,元件展現出線性的光響應特性,且可觀察到高達1300 的光暗電流比。
本研究亦將陽極氧化技術應用於在二氧化矽層上形成氧化鋁堆疊層,構築金屬/氧化鋁/二氧化矽/碳化矽金氧半結構。氧化鋁的製備方法包括熱蒸鍍後陽極氧化與原子層沉積。除了陽極氧化方法外,亦透過重複噴霧式間歇水合氧化法形成高品質的二氧化矽層。透過電流–電壓與電容–電壓等量測,比較不同製程條件下碳化矽基元件的電性特徵。實驗結果顯示,採用熱蒸鍍後陽極氧化製得的氧化鋁與重複噴霧式間歇水合氧化法製得的二氧化矽層,可實現介面陷阱密度低至2×10^11cm^−2eV^−1,具有較小的平帶電壓偏移與低漏電流特性。
最後,研究亦探討了閘極堆疊金氧半元件的記憶行為特性。實驗結果顯示,金屬/氧化鋁/(陽極氧化) 二氧化矽/碳化矽金氧半結構具有良好的記憶特性。在可靠度測試中,元件在100 次讀寫操作下可維持穩定的狀態0與狀態1電容。另外在暫態電流測試下,元件的暫態電流在1500次讀寫操作下,依舊可維持明顯的電流增益。並在寫入測試下,維持穩定電容間距達150秒。這些優異的成果展現碳化矽金氧半元件在記憶體領域的開發潛力。本研究亦輔以TCAD 模擬,以進一步分析電子濃度分佈、電場變化、電容–電壓特性曲線之漂移行為,以及暫態電流之響應特性,以全面探討元件在不同製程條件下之電性表現。
zh_TW
dc.description.abstractThis paper primarily investigates the process and application of anodizing aluminum oxide (Al2O3) and gate insulation layers on silicon carbide-substrates. Initially,the study examines the influence of UVC illumination on the anodization process. It is found that anodization under UVC lamp (ANOUVC) facilitates more holes generation in the SiC substrate, thereby enhancing the anodization current and facilitating the growth of SiO2- layers. This method successfully grew SiO2 layers up to 16 nm thick with good uniformity.
Furthermore, this research explores the characteristics of MIS devices with SiO2 formed by using Intermittent Spray Hydrated Oxidation (ISHO) and its- revised version of Intermittent Spray Hydrated Oxidation with Repetitive- Sprays (ISHO(r)). The results demonstrate that the ISHO(r) process can form uniform SiO2 with a thickness of 3∼ 6 nm, with low reverse leakage current. Interface characterization reveals that SiO2 grown by ISHO(r) has interface trap density (Dit) as low as 5×10^11 cm^−2eV^−1 at the SiO2/SiC interface. Under various UV light intensities at -6 V, the device exhibits linear responsivity with a photo-to-dark-current-ratio (PDCR) of 1300. The- anodization process is also applied to form Al2O3 stacking layers on the SiO2 layer, fabricating Al/Al2O3/SiO2/SiC(n) MOS structures. Two methods were used for Al2O3 formation, anodization after thermal- evaporation and atomic layer deposition (ALD). Besides the anodization process, Intermittent Spray Hydrated Oxidation with Repetitive Sprays is also used to form the SiO2 layer.
I–V and C–V measurements were conducted to compare the electrical- characteristics of SiC devices under different process conditions. It is found that Al2O3 formed by "anodization after thermal evaporation" and SiO2 formed by ISHO(r), could produce interface trap density (Dit) as low as 2×10^11 cm^−2eV^−1 in addition to less flatband shift and low leakage.
Finally, the memory characteristics of gate-stacking MOS devices were investigated. It is observed that Al/Al2O3/“ANO” SiO2/SiC(n) MOS structures exhibit good memory characteristics. In reliability tests, the device maintained stable capacitance for both state 0 and state 1 under 100 read/write operations. Furthermore, during transient current measurements, the device exhibited consistent current ratio even after 1500 read/write cycles. In the C–t retention test, a stable capacitance window was sustained for up to 150 seconds. These outstanding results demonstrate the potential of SiC-based MOS devices in memory applications. This study is further supported by TCAD simulations to analyze electron concentration distribution, electric field variation, the shift behavior of capacitance–voltage (C–V) characteristics, and transient current response. These analyses provide a comprehensive understanding of the device’s electrical performance under various process conditions.
en
dc.description.provenanceSubmitted by admin ntu (admin@lib.ntu.edu.tw) on 2025-07-18T16:06:19Z
No. of bitstreams: 0
en
dc.description.provenanceMade available in DSpace on 2025-07-18T16:06:19Z (GMT). No. of bitstreams: 0en
dc.description.tableofcontentsVerification Letter from the Oral Examination Committee . . . . . . . . . i
Acknowledgements . . . . . . . . . . . . . . . . . . . . . . . . . . . iii
摘要 . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . .v
Abstract. . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . vii
Contents. . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . ix
Figure Captions. . . . . . . . . . . . . . . . . . . . . . . . . . . . xiii
Table Captions . . . . . . . . . . . . . . . . . . . . . . . . . . . . .xix
Chapter 1 Introduction . . . . . . . . . . . . . . . . . . . . . . . . . 1
1.1 Research Motivation . . . . . . . . . . . . . . . . . . . . . . . . 1
1.2 The trend of Silicon and Silicon Carbide based
devices and its challenges . . . . . . . . . . . . . . . . . . . . . . . 4
1.2.1 Introduction of high-K dielectrics . . . . . . . . . . . . . . . . 4
1.2.2 Aluminum oxide/Silicon oxide on Silicon carbide substrate . . . . . 5
1.2.3 Ways to grow silicon oxide on Silicon Carbide . . . . . . . . . . . 8
1.3 Anodization Process . . . . . . . . . . . . . . . . . . . . . . . . . 9
1.4 MIS structure . . . . . . . . . . . . . . . . . . . . . . . . . . . 11
1.5 Measurement method and TCAD simulation . . . . . . . . . . . . . . . 15
1.6 Organization of this work . . . . . . . . . . . . . . . . . . . . . 15
Chapter 2 SiO2 Oxidation Methodology on SiC(n) Substrate. . . . . . . . 31
2.1 SiO2 on SiC Substrate by Anodization under UVC Lamp Illuminations
(ANOUVC) and by Intermittent Spray Hydrated Oxidation (ISHO) . . . . . . 31
2.2 Intermittent Spray Hydrated Oxidation with Repetitive Sprays (ISHO(r)) . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 33
2.3 Interface Quality of Al/SiO2/SiC(n) MIS Structure . . . . . . . . . 33
2.3.1 MIS Structure: "ANOUVC" versus Intermittent Spray Hydrated
Oxidation . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 33
2.3.2 MIS Structure: "ISHO" with Repetitive Sprays (ISHO(r)). . . . . . 36
2.4 Summary . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 42
Chapter 3 Characterization of Al/Al2O3/SiO2/SiC Gate Stacking MOS Structure
. . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 65
3.1 Introduction . . . . . . . . . . . . . . . . . . . . . . . . . . . 65
3.2 Experiment . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 68
3.2.1 SiC(n) based MOS structure: Al2O3 stacking on "ANO" SiO2 . . . . . 68
3.2.2 SiC(n) based MOS structure:"ALD" Al2O3 stacking on "ANO" SiO2. . . 69
3.2.3 SiC(n) based MOS structure: Al2O3 stacking on "ISHO(r)" SiO2 . . . 69
3.3 Interface quality of MOS structure with (1) Al2O3 stacking on "ANO"
SiO2 and (2)ALD Al2O3 on "ANO" SiO2 . . . . . . . . . . . . . . . . . . 70
3.4 Interface quality of MOS structure with Al2O3 stacking on "ISHO(r)"
SiO2 . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 73
3.5 Summary . . . . . . . . . . . . .. . . . . . . . . . . . . . . . . . 75
Chapter 4 Memory Behaviors of Al/Al2O3/SiO2/SiC(n) Gate Stacking MOS
Structure . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 91
4.1 Introduction . . . . . . . . . . . . . . . . . . . . . . . . . . . 91
4.2 Experimental . . . . . . . . . . . . . . . . . . . . . . . . . . . 92
4.2.1 MOS structure of Al/Al2O3 stacking/SiO2/SiC(n) (EOT=14 nm) . . . 92
4.2.2 MOS structure of Al/Al2O3 stacking/SiO2/SiC(n) (EOT=18.2 nm) . . 93
4.3 Memory operation: Al/Al2O3 stacking/SiO2/SiC(n) MOS (EOT=14
nm) . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 94
4.4 Memory operation: Al/Al2O3 stacking/SiO2/SiC(n) MOS (EOT=18.2
nm) . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 97
4.5 Summary . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 99
Chapter 5 Conclusion and Future Work . . . . . . . . . . . . . . . . 121
5.1 Conclusion . . . . . . . . . . . . . . . . . . . . . . . . . . . 121
5.2 Future Works . . . . . . . . . . . . . . . . . . . . . . . . . . 122
References . . . . . . . . . . . . . . . . . . . . . . . . . . . . . 127
Appendix A — Further Discussion of Chapter 2 . . . . . . . . . . . . 131
A.1 SiC(n) MIS device formed by ISHO(r) . . . . . . . . . . . . . . 131
-
dc.language.isoen-
dc.subjectMIS 元件zh_TW
dc.subject重覆噴霧式間歇水合氧化法zh_TW
dc.subject陽極氧化zh_TW
dc.subject介面缺陷zh_TW
dc.subjectMOS 元件zh_TW
dc.subject氧化鋁堆疊zh_TW
dc.subjectInterface trapsen
dc.subjectMOS deviceen
dc.subjectMIS deviceen
dc.subjectAl2O3 stackingen
dc.subjectISHO(r)en
dc.subjectAnodizationen
dc.title碳化矽金氧半結構之二氧化矽氧化方法暨介面與 記憶行為特性研究zh_TW
dc.titleSiO2 Oxidation Methodology and Characteristics of Interface and Memory Behaviors in Al/Al2O3/SiO2/SiC(n) MOS Structureen
dc.typeThesis-
dc.date.schoolyear113-2-
dc.description.degree碩士-
dc.contributor.oralexamcommittee吳幼麟;李坤彥zh_TW
dc.contributor.oralexamcommitteeYou-Lin Wu;Kung-Yen Leeen
dc.subject.keyword氧化鋁堆疊,MIS 元件,MOS 元件,介面缺陷,陽極氧化,重覆噴霧式間歇水合氧化法,zh_TW
dc.subject.keywordAl2O3 stacking,MIS device,MOS device,Interface traps,Anodization,ISHO(r),en
dc.relation.page135-
dc.identifier.doi10.6342/NTU202501320-
dc.rights.note同意授權(限校園內公開)-
dc.date.accepted2025-06-27-
dc.contributor.author-college電機資訊學院-
dc.contributor.author-dept電子工程學研究所-
dc.date.embargo-lift2025-07-19-
顯示於系所單位:電子工程學研究所

文件中的檔案:
檔案 大小格式 
ntu-113-2.pdf
授權僅限NTU校內IP使用(校園外請利用VPN校外連線服務)
16.78 MBAdobe PDF
顯示文件簡單紀錄


系統中的文件,除了特別指名其著作權條款之外,均受到著作權保護,並且保留所有的權利。

社群連結
聯絡資訊
10617臺北市大安區羅斯福路四段1號
No.1 Sec.4, Roosevelt Rd., Taipei, Taiwan, R.O.C. 106
Tel: (02)33662353
Email: ntuetds@ntu.edu.tw
意見箱
相關連結
館藏目錄
國內圖書館整合查詢 MetaCat
臺大學術典藏 NTU Scholars
臺大圖書館數位典藏館
本站聲明
© NTU Library All Rights Reserved